微纳米Ti2AlC增强TiAl复合材料高温强韧化机制 |
| 陈占兴, 王玉鹏, 荣光飞, 张新房, 马腾飞, 王晓红, 邢秋玮, 朱冬冬 |
|
High-Temperature Strengthening and Toughening Mechanisms of Micro-Nano Ti2AlC Reinforced TiAl Composites |
| CHEN Zhanxing, WANG Yupeng, RONG Guangfei, ZHANG Xinfang, MA Tengfei, WANG Xiaohong, XING Qiuwei, ZHU Dongdong |
| 图5 1300℃烧结TiAl合金及不同温度烧结添加0.5%GO的Ti2AlC颗粒增强TiAl复合材料的片层团尺寸及片层间距的统计结果 |
| Fig.5 Statistical results of lamellar colony size and lamellar space for TiAl alloy sintered at 1300oC and Ti2AlC reinforced TiAl composites with 0.5%GO addition sintered at different temperatures |
|