多场耦合侵蚀下环保Ag/Ti2SnC复合电接触材料的微/纳米力学行为及微结构演变 |
| 丁宽宽, 丁健翔, 张凯歌, 白忠臣, 张培根, 孙正明 |
|
Micro/Nano-Mechanical Behavior and Microstructure Evolution of Eco-Friendly Ag/Ti2SnC Composite Electrical Contacts Under Multi-Field Coupled Erosion |
| DING Kuankuan, DING Jianxiang, ZHANG Kaige, BAI Zhongchen, ZHANG Peigen, SUN Zhengming |
| 图11 Ag/10%Ti2SnC复合材料中区域α和区域β的SEM像和元素面分布 |
| Fig.11 SEM images and element mapping distributions of area α (a) and area β (b) in Ag/10%Ti2SnC contact |
|