超高速激光原位熔覆Ti(C, B)/Ni60A复合涂层的界面特征与表面磨损机理 |
| 徐一斐, 张楠, 许培鑫, 杜博睿, 史华, 王淼辉 |
|
Interfacial Characterization and Surface Wear Mechanism of Ti(C, B)/Ni60A Composite Coating Prepared by In Situ Extra High-Speed Laser Cladding |
| XU Yifei, ZHANG Nan, XU Peixin, DU Borui, SHI Hua, WANG Miaohui |
| 图5 Ti(C, B)/Ni60A复合涂层、Ni60A涂层和H13钢的表面磨损形貌 |
| Fig.5 Surface wear morphologies of Ti(C, B)/Ni60A composite coating (a), Ni60A coating (b), and H13 steel (c) |
|