脉冲电流作用下Pb-Al合金的液-固分相过程
|
|
李彦强, 赵九洲, 江鸿翔, 张丽丽, 何杰
|
Liquid-Solid Phase Separation Process of Pb-Al Alloy Under the Effect of Electric Current Pulses
|
|
LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, ZHANG Lili, HE Jie
|
|
表1 Pb-Al体系的热物性参数[28]
|
Table 1 Thermophysical property parameters of Pb-Al system[28]
|
|
| Parameter | Value | Unit |
|---|
| Dynamic viscosity of Pb | 0.0004636exp(1036.7 / T) | Pa·s | | Thermal conductivity of liquid Pb | 15.88 | W·m-1·K-1 | | Density of liquid Pb | 10670 - 1.32(T - 600.4) | kg·m-3 | | Density of solid Al | 2700 | kg·m-3 | | Specific heat of liquid Pb | 127.61 | J·kg-1·K-1 | | Latent heat of solidification of Pb | 24700 | J·kg-1 | | Electrical conductivity of liquid Pb | (0.0479T + 66.6)-1 | 10-8 S·m-1 | | Electrical conductivity of solid Al | [15(exp(0.00057T)–1)]-1 | 10-8 S·m-1 |
|
|
|