脉冲电流作用下Pb-Al合金的液-固分相过程
李彦强, 赵九洲, 江鸿翔, 张丽丽, 何杰

Liquid-Solid Phase Separation Process of Pb-Al Alloy Under the Effect of Electric Current Pulses
LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, ZHANG Lili, HE Jie
图13 峰值电流密度为8 × 108 A/m2时凝固界面前沿中心轴线处,ΔT、S、I、N、R¯沿z轴变化曲线,及位置No.1~6处Al粒子的半径分布函数
Fig.13 Curves of ΔT, S, I, N, and R¯vsz for Pb-0.15Al alloys solidified under the effect of ECPs (a, b), and the radius distribution function (f) of the Al-rich particles at the positions of Nos.1~6 as marked in Figs.13a and b (c) with jmax = 8 × 108 A/m2 (Fig.13b is the local enlargement of Fig.13a)