脉冲电流作用下Pb-Al合金的液-固分相过程
李彦强, 赵九洲, 江鸿翔, 张丽丽, 何杰

Liquid-Solid Phase Separation Process of Pb-Al Alloy Under the Effect of Electric Current Pulses
LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, ZHANG Lili, HE Jie
图12 不同jmax条件下Pb-0.15Al合金中心轴线处熔体温度(T)、S及I沿z轴变化曲线
Fig.12 Curves of T, S and Ivsz with jmax values being 0 A/m2 (a), 4 × 108 A/m2 (b), 6 × 108 A/m2 (c), and 8 × 108 A/m2 (d), respectively (II—Al-rich particles' nucleation rate at the moment of j=jmax; III—Al-rich particles' nucleation rate during the period ofj=0. The parameter with subscript “max” refers to the maximum value for the corresponding parameter)