脉冲电流作用下Pb-Al合金的液-固分相过程
|
|
李彦强, 赵九洲, 江鸿翔, 张丽丽, 何杰
|
Liquid-Solid Phase Separation Process of Pb-Al Alloy Under the Effect of Electric Current Pulses
|
|
LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, ZHANG Lili, HE Jie
|
|
图6 不施加脉冲电流时Pb-0.15Al合金凝固界面前沿中心轴线处基体熔体过冷度()、过饱和度(),Al粒子形核率()、数量密度()及平均半径()沿z轴变化曲线
|
Fig.6 Supercooling () and supersaturation () of the matrix melt, and nucleation rate (), number density (), and average radius () of the Al-rich particles in front of the solidification interface along the central axis for Pb-0.15Al alloys solidified without ECPs (a), and the enlargement of the microstructure evolution in the nucleation region of the Al-rich particles (b)
|
|
|
|
|