脉冲电流作用下Pb-Al合金的液-固分相过程 |
| 李彦强, 赵九洲, 江鸿翔, 张丽丽, 何杰 |
|
Liquid-Solid Phase Separation Process of Pb-Al Alloy Under the Effect of Electric Current Pulses |
| LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, ZHANG Lili, HE Jie |
| 图3 不同jmax条件下Pb-0.15Al合金凝固组织中Al粒子的二维尺寸分布 |