A2BTi型磁性功能合金相稳定性、磁性与力学性能的第一性原理计算和实验研究 |
| 杨谨菡, 闫海乐, 刘昊轩, 赵莹, 杨一俏, 赵骧, 左良 |
|
Phase Stability, Magnetism, and Mechanical Properties of A2BTi: First-Principles Calculations and Experimental Studies |
| YANG Jinhan, YAN Haile, LIU Haoxuan, ZHAO Ying, YANG Yiqiao, ZHAO Xiang, ZUO Liang |
| 图3 Co2NiTi、Fe2NiTi和Ni2CoTi室温XRD谱和背散射电子(BSE)像 |
| Fig.3 XRD spectra (a1-c1) and backscattered electron (BSE) images (a2-c2) for Co2NiTi (a1, a2), Fe2NiTi (b1, b2), and Ni2CoTi (c1, c2) alloys at room temperature (Insets in Figs.3a1, b1, and c1 show the crystal structural models of the matrix phase and the precipitated phases of Co2NiTi, Fe2NiTi, and Ni2CoTi alloys, respectively) |
|