A2BTi型磁性功能合金相稳定性、磁性与力学性能的第一性原理计算和实验研究 |
| 杨谨菡, 闫海乐, 刘昊轩, 赵莹, 杨一俏, 赵骧, 左良 |
|
Phase Stability, Magnetism, and Mechanical Properties of A2BTi: First-Principles Calculations and Experimental Studies |
| YANG Jinhan, YAN Haile, LIU Haoxuan, ZHAO Ying, YANG Yiqiao, ZHAO Xiang, ZUO Liang |
| 图2 平均原子磁矩与平均价电子浓度分布图 |
| Fig.2 Distribution diagram of average atomic magnetic moment and average valence electron concentration (VEC) (Hollow dots and solid dots represent the alloy in which L21 phase is and isn't the most stable phase, respectively) |
|