黏性烧结过程的相场模拟
郭松源, 柳文波, 杨庆成, 戚晓勇, 恽迪

Phase Field Simulation of Viscous Sintering
GUO Songyuan, LIU Wenbo, YANG Qingcheng, QI Xiaoyong, YUN Di
表1 175℃下尼龙12的物理参数[12,23]
Table 1 Physical parameters of nylon 12 (PA12) at 175oC[12,23]
Physical parameterValueUnitRef.
ρliquid840kg·m-3[23]
ρgas0.806kg·m-3[23]
μliquid400pa·s[23]
μgas2.47pa·s[23]
M1 × 10-6-[12]
Δx0.825nm
σ0.03N·m-1[23]