激光束空域形态对激光定向能量沉积316L不锈钢热输运影响的数值模拟 |
| 任松, 吴家柱, 张屹, 张大斌, 曹阳, 尹存宏 |
|
Numerical Simulation on Effects of Spatial Laser Beam Profiles on Heat Transport During Laser Directed Energy Deposition of 316L Stainless Steel |
| REN Song, WU Jiazhu, ZHANG Yi, ZHANG Dabin, CAO Yang, YIN Cunhong |
| 图6 超Gaussian形态(SGP1,K = 4.2)作用下不同功率时沉积道形貌的数值模拟结果与实验结果 |
| Fig.6 Experimental and simulated results at laser powers of 600 W (a), 700 W (b), and 800 W(c) under the action of SGP1 |
|