闪速加热对2000 MPa级热成形钢显微组织和力学性能的影响 |
| 谢泽东, 丁灿灿, 温鹏宇, 罗海文 |
|
Effect of Flash Heating on Microstructure and Mechanical Properties of 2000 MPa Hot Stamping Steel |
| XIE Zedong, DING Cancan, WEN Pengyu, LUO Haiwen |
| 图7 冷轧板在850、900和950℃闪速加热5 s后的微观组织演变示意图 |
| Fig.7 Schematic of the microstructural evolutions of cold-rolled steel during the flash heating at 850, 900, and 950oC for 5 s |
|