闪速加热对2000 MPa级热成形钢显微组织和力学性能的影响 |
| 谢泽东, 丁灿灿, 温鹏宇, 罗海文 |
|
Effect of Flash Heating on Microstructure and Mechanical Properties of 2000 MPa Hot Stamping Steel |
| XIE Zedong, DING Cancan, WEN Pengyu, LUO Haiwen |
| 图6 FH950和CH950样品的EBSD质量图和相分布叠加图、FH950样品Auger能谱、不同热成形工艺样品的XRD谱及残余奥氏体体积分数 |
| Fig.6 EBSD image quality map overlapped with phase distribution on the microstructures of FH950 (a) and CH950 (b) specimens; Auger mapping of C, Mn, and Cr distributions in retained austenite (RA, green regions) in FH950 specimen (c); XRD spectra (d) and RA volume fractions (e) of the specimens subjected to both the conventional and flash heating processes |
|