表1 2种低碳马氏体不锈钢的化学成分 (mass fraction / %)
Table 1 Chemical compositions of two low-carbon martensitic stainless steels
SteelCCrNiMoSiMnCuPSFe

0Cu

3Cu

0.051

0.056

12.87

13.03

4.06

4.12

0.47

0.48

0.43

0.51

0.68

0.66

0.01

2.82

0.005

0.005

0.0041

0.0050

Bal.

Bal.