含3%Cu低碳马氏体不锈钢0Cr13Ni4Mo的显微组织及耐腐蚀性能
杨彬彬, 宋元元, 郝龙, 姜海昌, 戎利建

Microstructure and Corrosion Resistance of Low-Carbon Martensitic Stainless Steel 0Cr13Ni4Mo with 3%Cu Addition
YANG Binbin, SONG Yuanyuan, HAO Long, JIANG Haichang, RONG Lijian
图9 3Cu钢经过500℃保温2 h回火后Fe、Cr、Ni、Mn、Mo、C和Cu原子的三维空间分布图,3%C原子和15%Cu原子的等浓度面分布图以及相应团簇的成分分布
Fig.9 Atom distribution maps of Fe, Cr, Ni, Mn, Mo, C, and Cu in 3Cu stainless steel 500oC tempered for 2 h (a), isoconcentration surface distribution of 3%C (atomic fraction) and corresponding C clusters distribution (b), and isoconcentration surface distribution of 15%Cu (atomic fraction) and corresponding Cu cluster distribution (c)