含3%Cu低碳马氏体不锈钢0Cr13Ni4Mo的显微组织及耐腐蚀性能 |
杨彬彬, 宋元元, 郝龙, 姜海昌, 戎利建 |
Microstructure and Corrosion Resistance of Low-Carbon Martensitic Stainless Steel 0Cr13Ni4Mo with 3%Cu Addition |
YANG Binbin, SONG Yuanyuan, HAO Long, JIANG Haichang, RONG Lijian |
图1 不同热处理工艺下0Cu钢和3Cu钢基体组织的SEM像 |
Fig.1 SEM images of 0Cu (a-c) and 3Cu (d-f) steels after different heat treatments (a, d) solution treated at 1050oC (b, e) tempered at 400oC (c, f) tempered at 500oC |
![]() |