B微合金化对CoNiV中熵合金微观组织和力学性能的影响及其机理 |
|||||||||
| 南勇, 关旭, 闫海乐, 唐帅, 贾楠, 赵骧, 左良 | |||||||||
|
Effect and Mechanism of B Microalloying on the Microstructure and Mechanical Properties of CoNiV Medium-Entropy Alloy |
|||||||||
| NAN Yong, GUAN Xu, YAN Haile, TANG Shuai, JIA Nan, ZHAO Xiang, ZUO Liang | |||||||||
| 表2 CoNiV和(CoNiV)99.8B0.2合金的硬度比值 |
|||||||||
| Table 2 Ratios of hardness measured at different regions of CoNiV and (CoNiV)99.8B0.2 alloys |
|||||||||
|
|||||||||