B微合金化对CoNiV中熵合金微观组织和力学性能的影响及其机理 |
| 南勇, 关旭, 闫海乐, 唐帅, 贾楠, 赵骧, 左良 |
|
Effect and Mechanism of B Microalloying on the Microstructure and Mechanical Properties of CoNiV Medium-Entropy Alloy |
| NAN Yong, GUAN Xu, YAN Haile, TANG Shuai, JIA Nan, ZHAO Xiang, ZUO Liang |
| 图2 CoNiV、(CoNiV)99.9B0.1和(CoNiV)99.8B0.2合金的XRD谱、相分布图与晶体学取向分布图 |
| Fig.2 XRD spectra (a1-a3), phase distribution maps (fcc phase colored in red) overlapped with Σ3 (white), Σ5 (green), Σ7 (blue), and Σ9 (purple) coincidence site lattice (CSL) boundaries (b1-b3), and orientation maps represented by inverse pole figures (IPFs) (c1-c3) for CoNiV (a1-c1), (CoNiV)99.9B0.1 (a2-c2), and (CoNiV)99.8B0.2 (a3-c3) alloys (RD—rolling direction, ND—normal direction, LD—loading direction) |
|