B微合金化对CoNiV中熵合金微观组织和力学性能的影响及其机理 |
| 南勇, 关旭, 闫海乐, 唐帅, 贾楠, 赵骧, 左良 |
|
Effect and Mechanism of B Microalloying on the Microstructure and Mechanical Properties of CoNiV Medium-Entropy Alloy |
| NAN Yong, GUAN Xu, YAN Haile, TANG Shuai, JIA Nan, ZHAO Xiang, ZUO Liang |
| 图1 CoNiV、(CoNiV)99.9B0.1和(CoNiV)99.8B0.2合金的室温静态拉伸力学性能 |
| Fig.1 Static tensile mechanical properties of CoNiV, (CoNiV)99.9B0.1, and (CoNiV)99.8B0.2 alloys at room temperature (a) engineering stress-strain curves (b) true stress-true strain curves (c) strain-hardening rate curves |
|