TiAl基合金与GH3039合金摩擦-扩散双重焊焊合区过渡相的形成、结构与原位开裂 |
| 杜随更, 王松林, 胡弘毅 |
|
Formation, Structure, and In Situ Cracking of Intermediate Phases in the Friction-Diffusion Double Welding Zone Between TiAl-Based Alloy and GH3039 Alloy |
| DU Suigeng, WANG Songlin, HU Hongyi |
| 图5 |
| Fig.5 Atomic projection STEM image (a) and selected area electron diffraction (SAED) pattern (b) of Al3NiTi2 phase in region R1 in Fig.3 (d—spacing) |
|