热处理调控 α + β 两相钛合金板材的力学及导电性能 |
| 张术钱, 马英杰, 王倩, 齐敏, 黄森森, 雷家峰, 杨锐 |
|
Mechanical Properties and Electrical Conductivity of α + β Titanium Alloy Sheet Regulated by Heat Treatment |
| ZHANG Shuqian, MA Yingjie, WANG Qian, QI Min, HUANG Sensen, LEI Jiafeng, YANG Rui |
| 图12 Ti-6Al-3Mo-2V-1Cr-2Sn-2Zr合金板材经不同温度退火后α相RD和TD的反极图以及基面和柱面滑移的等Schmidt因子分布图 |
| Fig.12 Inverse pole figures of RD and TD of α phase in Ti-6Al-3Mo-2V-1Cr-2Sn-2Zr alloy sheet after annealing at 800oC (a), 900oC (b), 920oC (c), 950oC (d), and 1000oC (e); and inverse pole figures along with isocurves of the maximum Schmidt factor for orientations in which basal slip (f) and prismatic slip (g) |
|