热处理调控 α + β 两相钛合金板材的力学及导电性能 |
| 张术钱, 马英杰, 王倩, 齐敏, 黄森森, 雷家峰, 杨锐 |
|
Mechanical Properties and Electrical Conductivity of α + β Titanium Alloy Sheet Regulated by Heat Treatment |
| ZHANG Shuqian, MA Yingjie, WANG Qian, QI Min, HUANG Sensen, LEI Jiafeng, YANG Rui |
| 图11 沿Ti-6Al-3Mo-2V-1Cr-2Sn-2Zr合金板材轧向(RD)和横向(TD) α相不同滑移系的Schmidt因子分布 |
| Fig.11 Schmidt factor distributions along the RD (a) and TD (b) in Ti-6Al-3Mo-2V-1Cr-2Sn-2Zr alloy sheet with different slip systems of α phase |
|