热处理调控 α + β 两相钛合金板材的力学及导电性能
张术钱, 马英杰, 王倩, 齐敏, 黄森森, 雷家峰, 杨锐

Mechanical Properties and Electrical Conductivity of α + β Titanium Alloy Sheet Regulated by Heat Treatment
ZHANG Shuqian, MA Yingjie, WANG Qian, QI Min, HUANG Sensen, LEI Jiafeng, YANG Rui
图4 不同温度退火空冷后Ti-6Al-3Mo-2V-1Cr-2Sn-2Zr合金板材显微组织的SEM像
Fig.4 Low (a-f) and high (a1-f1) magnified SEM images of air-cooled Ti-6Al-3Mo-2V-1Cr-2Sn-2Zr alloy sheet after annealing at 800oC (a, a1), 850oC (b, b1), 900oC (c, c1), 920oC (d, d1), 950oC (e, e1), and 1000oC (f, f1) for 1 h (αs—secondary α phase, αGB—grain boundary α phase, βt—β transformed phase)