热处理调控 α + β 两相钛合金板材的力学及导电性能 |
| 张术钱, 马英杰, 王倩, 齐敏, 黄森森, 雷家峰, 杨锐 |
|
Mechanical Properties and Electrical Conductivity of α + β Titanium Alloy Sheet Regulated by Heat Treatment |
| ZHANG Shuqian, MA Yingjie, WANG Qian, QI Min, HUANG Sensen, LEI Jiafeng, YANG Rui |
| 图3 Ti-6Al-3Mo-2V-1Cr-2Sn-2Zr合金板材轧向-法向(RD-ND)面α相的取向成像图以及α相和β相的极图 |
| Fig.3 Orientation imaging map of α phase in RD-ND plane (a), and pole figures of α phase (b) and β phase (c) in Ti-6Al-3Mo-2V-1Cr-2Sn-2Zr alloy sheet |
|