B、Zr复合添加对IN718高温合金流动性的影响
介子奇, 刘鼎元, $\boxed{\hbox{张军}}$

Effect of Combined Addition of B and Zr on the Fluidity of IN718 Superalloy
JIE Ziqi, LIU Dingyuan, $\boxed{\hbox{Zhang Jun}}$
表2 浇铸温度为1470℃时,不同Zr和B含量IN718合金的流动长度
Table 2 Statistical data of flow lengths for IN718 at the pouring temperature of 1470oC
AlloyAverage length / mmStandard deviation / %
12757.6
24168.3
34219.5
45239.6