减少钛合金表面氧化的阴极电保护激光加工的研究 |
| 梁良, 姜治康, 谭欢恒, 陈健, 姜长城, 易根苗, 林新贵 |
|
Study on Cathodic Protection Assisted Laser Processing (CPALP) for Reducing Titanium Alloy Surface Oxidation |
| LIANG Liang, JIANG Zhikang, TAN Huanheng, CHEN Jian, JIANG Changcheng, YI Genmiao, LIN Xingui |
| 图4 不同电解液和工作电流下加工区域的O含量 |
| Fig.4 Oxygen contents in the processing area under different electrolytes and working currents |
|