减少钛合金表面氧化的阴极电保护激光加工的研究 |
| 梁良, 姜治康, 谭欢恒, 陈健, 姜长城, 易根苗, 林新贵 |
|
Study on Cathodic Protection Assisted Laser Processing (CPALP) for Reducing Titanium Alloy Surface Oxidation |
| LIANG Liang, JIANG Zhikang, TAN Huanheng, CHEN Jian, JIANG Changcheng, YI Genmiao, LIN Xingui |
| 图3 不同的工作电流和电解液中加工区域的表面微观形貌 |
| Fig.3 Surface micromorphologies of the machining area under different working currents of 0 mA (a, e, i), 300 mA (b, f, j), 600 mA (c, g, k), and 900 mA (d, h, l) and electrolytes of A (a-d), B (e-h), and C (i-l) (wO—mass fraction of oxygen) |
|