纵向静磁场对DD98M合金定向凝固微观组织与偏析的影响 |
| 刘翔, 王英豪, 张小新, 陈超越, 孟杰, 余建波, 王江, 任忠鸣 |
|
Influence of Longitudinal Static Magnetic Field on Microstructure and Microsegregation During Directional Solidification of DD98M Alloy |
| LIU Xiang, WANG Yinghao, ZHANG Xiaoxin, CHEN Chaoyue, MENG Jie, YU Jianbo, WANG Jiang, REN Zhongming |
| 图11 枝晶尺度上不同磁场强度下定向凝固DD98M合金中Al、Ta、Co、W元素的溶质浓度分布曲线 |
| Fig.11 Concentration profiles of Al (a), Ta (b), Co (c), and W (d) of directionally solidified DD98M alloy under different B on dendritic scale (CS—solid composition, C0—original composition, CS / C0—relative solute concentration, fs—solid fraction) |
|