纵向静磁场对DD98M合金定向凝固微观组织与偏析的影响 |
| 刘翔, 王英豪, 张小新, 陈超越, 孟杰, 余建波, 王江, 任忠鸣 |
|
Influence of Longitudinal Static Magnetic Field on Microstructure and Microsegregation During Directional Solidification of DD98M Alloy |
| LIU Xiang, WANG Yinghao, ZHANG Xiaoxin, CHEN Chaoyue, MENG Jie, YU Jianbo, WANG Jiang, REN Zhongming |
| 图8 磁场对枝晶干与枝晶间γ'相尺寸的影响 |
| Fig.8 Relationship between the size of γ' phase and B |
|