纵向静磁场对DD98M合金定向凝固微观组织与偏析的影响 |
| 刘翔, 王英豪, 张小新, 陈超越, 孟杰, 余建波, 王江, 任忠鸣 |
|
Influence of Longitudinal Static Magnetic Field on Microstructure and Microsegregation During Directional Solidification of DD98M Alloy |
| LIU Xiang, WANG Yinghao, ZHANG Xiaoxin, CHEN Chaoyue, MENG Jie, YU Jianbo, WANG Jiang, REN Zhongming |
| 图4 抽拉速率100 μm/s时磁场强度(B)对一次枝晶间距(λ)的影响 |
| Fig.4 Effect of B on the primary dendrite arm spacing (λ) under withdraw rate 100 μm/s |
|