纵向静磁场对DD98M合金定向凝固微观组织与偏析的影响 |
| 刘翔, 王英豪, 张小新, 陈超越, 孟杰, 余建波, 王江, 任忠鸣 |
|
Influence of Longitudinal Static Magnetic Field on Microstructure and Microsegregation During Directional Solidification of DD98M Alloy |
| LIU Xiang, WANG Yinghao, ZHANG Xiaoxin, CHEN Chaoyue, MENG Jie, YU Jianbo, WANG Jiang, REN Zhongming |
| 图1 强磁场液态金属冷却(LMC) Bridgman定向凝固装置示意图 |
| Fig.1 Schematic of liquid metal cooling (LMC) Bridgman directional solidification apparatus with a high static magnetic field (1—temperature control system; 2—thermocouples; 3—heating element; 4—heating element protection cover; 5—double pass corundum tube; 6—alloy; 7—superconductor magnet; 8—LMC seal; 9—Ga-In-Sn liquid metal; 10—water cooling protection cover water outlet; 11—LMC water outlet; 12—drawbar; 13—water cooling protection cover water inlet; 14—bumper; 15—LMC water inlet) |
|