强磁场下过冷Cu-Co/Cu-Co-Fe合金的凝固组织和摩擦性能 |
| 魏晨, 王军, 闫育洁, 范嘉懿, 李金山 |
|
Solidification Microstructure and Wear Properties of Undercooled Cu-Co/Cu-Co-Fe Alloys Under a High Magnetic Field |
| WEI Chen, WANG Jun, YAN Yujie, FAN Jiayi, LI Jinshan |
| 图9 不同磁场强度及不同过冷度下Cu50Co50中富Co相以及Cu52Fe24Co24合金中富(Co, Fe)相的硬度 |
| Fig.9 Microhardnesses of the Co-rich phase in Cu50Co50 and the Co, Fe-rich phase in Cu52Fe24Co24 alloys under different ΔT and magnetic fields |
|