强磁场下过冷Cu-Co/Cu-Co-Fe合金的凝固组织和摩擦性能 |
| 魏晨, 王军, 闫育洁, 范嘉懿, 李金山 |
|
Solidification Microstructure and Wear Properties of Undercooled Cu-Co/Cu-Co-Fe Alloys Under a High Magnetic Field |
| WEI Chen, WANG Jun, YAN Yujie, FAN Jiayi, LI Jinshan |
| 图5 不同磁场强度及不同过冷度下Cu52Co24Fe24合金磨损表形貌 |
| Fig.5 Worn surfaces morphologies of Cu52Co24Fe24 alloy at different ΔT and magnetic fields (a-f) and corresponding enlarged images of boxed regions (a1-f1) |
|