巨磁致伸缩Fe-Ga合金薄带的抑制剂与二次再结晶行为 |
| 翟欣雅, 和正华, 沙玉辉, 朱晓飞, 李锋, 陈立佳, 左良 |
|
Inhibitor and Secondary Recrystallization Behavior of Giant Magnetostriction of Fe-Ga Thin Sheet |
| ZHAI Xinya, HE Zhenghua, SHA Yuhui, ZHU Xiaofei, LI Feng, CHEN Lijia, ZUO Liang |
| 图12 Fe-Ga合金薄带中Goss晶粒的二次再结晶机制示意图 (a) primary recrystallization (b) onset of secondary recrystallization (c) process of secondary recrystallization |
| Fig.12 Schematics of mechanism of secondary recrystallization in Fe-Ga alloy thin sheet |
|