巨磁致伸缩Fe-Ga合金薄带的抑制剂与二次再结晶行为 |
| 翟欣雅, 和正华, 沙玉辉, 朱晓飞, 李锋, 陈立佳, 左良 |
|
Inhibitor and Secondary Recrystallization Behavior of Giant Magnetostriction of Fe-Ga Thin Sheet |
| ZHAI Xinya, HE Zhenghua, SHA Yuhui, ZHU Xiaofei, LI Feng, CHEN Lijia, ZUO Liang |
| 图6 Fe-Ga合金薄带在高温退火至不同温度时沿轧面恒φ2 = 45°的ODF截面图 |
| Fig.6 Constant φ2 = 45° sections of ODFs of Fe-Ga alloy thin sheet along the rolling plane during the heating process at annealing temperatures of 800oC (a), 850oC (b), 900oC (c), 950oC (d), and 1000oC (e) |
|