巨磁致伸缩Fe-Ga合金薄带的抑制剂与二次再结晶行为 |
| 翟欣雅, 和正华, 沙玉辉, 朱晓飞, 李锋, 陈立佳, 左良 |
|
Inhibitor and Secondary Recrystallization Behavior of Giant Magnetostriction of Fe-Ga Thin Sheet |
| ZHAI Xinya, HE Zhenghua, SHA Yuhui, ZHU Xiaofei, LI Feng, CHEN Lijia, ZUO Liang |
| 图2 Fe-Ga合金薄带初次再结晶析出相形貌的TEM像与EDS |
| Fig.2 TEM image (a) and EDS of precipitates NbC (b) and MnS (c) in Fe-Ga alloy thin sheet after primary recrystallization |
|