可降解Zn表面金属-多酚载药涂层骨生成和抗菌性能 |
| 林雪, 钱军余, 张文泰, 王鹏, 万国江 |
|
Osteogenic and Antibacterial Metal-Polyphenol Drug-Loaded Coating on Biodegradable Zinc for Orthopedic Implants Application |
| LIN Xue, QIAN Junyu, ZHANG Wentai, WANG Peng, WAN Guojiang |
| 图8 MC3T3-E1在不锈钢(SS)、Zn、TA/Met、Cu-TA/Met、Fe-TA/Met、Mg-TA/Met和Sr-TA/Met样品表面培养1 d后的荧光图像 |
| Fig.8 Fluorescence microscopy images of MC3T3-E1 cultured on stainless steel (SS) (a), Zn (b), TA/Met (c), Cu-TA/Met (d), Fe-TA/Met (e), Mg-TA/Met (f), and Sr-TA/Met (g) for 1 d |
|