可降解Zn表面金属-多酚载药涂层骨生成和抗菌性能 |
| 林雪, 钱军余, 张文泰, 王鹏, 万国江 |
|
Osteogenic and Antibacterial Metal-Polyphenol Drug-Loaded Coating on Biodegradable Zinc for Orthopedic Implants Application |
| LIN Xue, QIAN Junyu, ZHANG Wentai, WANG Peng, WAN Guojiang |
| 图3 TA/Met、Cu-TA/Met、Fe-TA/Met、Mg-TA/Met和Sr-TA/Met的高分辨XPS |
| Fig.3 High-resolution XPS of C1s (a), N1s (b), O1s (c), Zn2p (d), Cu2p, Fe2p, Mg2p, and Sr3d (e) of TA/Met, Cu-TA/Met, Fe-TA/Met, Mg-TA/Met, and Sr-TA/Met |
|