钛合金三次真空自耗电弧熔炼过程中的宏观偏析传递行为 |
| 郭杰, 黄立清, 吴京洋, 李俊杰, 王锦程, 樊凯 |
|
Evolution of Macrosegregation During Three-Stage Vacuum Arc Remelting of Titanium Alloys |
| GUO Jie, HUANG Liqing, WU Jingyang, LI Junjie, WANG Jincheng, FAN Kai |
| 图9 全部三次熔炼铸锭最终成分分布对比 |
| Fig.9 Comparisons of final concentration distributions of all triple remelting ingots (a) VAR1-A (b) VAR2-A (c) VAR2-D (d) VAR2-R (e) VAR3-A (f) VAR3-D-D (g) VAR3-D-R (h) VAR3-R-D (i) VAR3-R-R |
|