钛合金三次真空自耗电弧熔炼过程中的宏观偏析传递行为 |
| 郭杰, 黄立清, 吴京洋, 李俊杰, 王锦程, 樊凯 |
|
Evolution of Macrosegregation During Three-Stage Vacuum Arc Remelting of Titanium Alloys |
| GUO Jie, HUANG Liqing, WU Jingyang, LI Junjie, WANG Jincheng, FAN Kai |
| 图4 第二次熔炼过程中不同时刻下径向浓度分布曲线 |
| Fig.4 Radial concentration distribution curves at different time during the second remelting process (The extracted concentration positions are shown by horizontal lines in Fig.3) (a) comparisons of the three electrode placement results at 2200 s (b) comparisons of the three electrode placement results at 5080 s |
|