钛合金三次真空自耗电弧熔炼过程中的宏观偏析传递行为 |
| 郭杰, 黄立清, 吴京洋, 李俊杰, 王锦程, 樊凯 |
|
Evolution of Macrosegregation During Three-Stage Vacuum Arc Remelting of Titanium Alloys |
| GUO Jie, HUANG Liqing, WU Jingyang, LI Junjie, WANG Jincheng, FAN Kai |
| 图3 第二次熔炼时的溶质场及流场演化 |
| Fig.3 Solute distributions and liquid phase flow vectors in the ingot at 1000 s (a1-c1), 2200 s (a2-c2), 3800 s (a3-c3), 5080 s (a4-c4), 6520 s (a5-c5), 8520 s (a6-c6), and 9440 s (a7-c7) during the second smelting process (a1-a7) VAR2-A (b1-b7) VAR2-D (c1-c7) VAR2-R |
|