激光熔化沉积制备316L不锈钢的电化学腐蚀及空化腐蚀性能 |
| 蒋华臻, 彭爽, 胡琦芸, 王光义, 陈启生, 李正阳, 孙辉磊, 房佳汇钰 |
|
Corrosion and Cavitation Erosion Resistance of 316L Stainless Steels Produced by Laser Metal Deposition |
| JIANG Huazhen, PENG Shuang, HU Qiyun, WANG Guangyi, CHEN Qisheng, LI Zhengyang, SUN Huilei, FANG Jiahuiyu |
| 图14 经0.5和4 h空化腐蚀测试后No.2试样的表面形貌 |
| Fig.14 Topographies of sample No.2 after 0.5 h (a, b) and 4 h (c, d) of the cavitation test (a, c) SEM images (Inset in Fig.14c is the local magnified image) (b, d) images obtained by 3D white light interferometric surface topography |
|