激光熔化沉积制备316L不锈钢的电化学腐蚀及空化腐蚀性能 |
| 蒋华臻, 彭爽, 胡琦芸, 王光义, 陈启生, 李正阳, 孙辉磊, 房佳汇钰 |
|
Corrosion and Cavitation Erosion Resistance of 316L Stainless Steels Produced by Laser Metal Deposition |
| JIANG Huazhen, PENG Shuang, HU Qiyun, WANG Guangyi, CHEN Qisheng, LI Zhengyang, SUN Huilei, FANG Jiahuiyu |
| 图4 不同工艺参数下的激光熔化沉积316L (LMD-316L)不锈钢成形件致密度及相应的典型缺陷形貌图 |
| Fig.4 Relative densities of LMD-produced 316L (LMD-316L) SS fabricated by different process parameters and the representative defects images |
|