粉末冶金Inconel 718合金的热等静压成形和原始颗粒边界的消除 |
| 田晓生, 卢正冠, 徐磊, 吴杰, 杨锐 |
|
Hot Isostatic Densification of Inconel 718 Powder Alloy and Elimination of Prior Particle Boundaries |
| TIAN Xiaosheng, LU Zhengguan, XU Lei, WU Jie, YANG Rui |
| 图10 Inconel 718结构件标准热处理和特殊高温热处理试样拉伸断口形貌的SEM像 |
| Fig.10 SEM fractographs of tensile samples of Inconel 718 component (a) HT (b) SHT1 (c) SHT2 (d) SHT3 |
|