Effects of Overlapping Process on Grain Orientation and Microstructure of Nickel-Based Single-Crystal Superalloy DD491 Fabricated by Selective Laser Melting |
| ZHANG Zhenwu, LI Jikang, XU Wenhe, SHEN Muyu, QI Leiyi, ZHENG Keying, LI Wei, WEI Qingsong |
| 图15 熔池内[001]、[010]、[100]晶体生长方向示意图 |
| Fig.15 Schematic of the [001], [010], and [100] grain growth directions in the melt pool (θ—the angle between |
|