搭接工艺对选区激光熔化镍基单晶高温合金DD491晶体取向与微观组织的影响 |
| 张振武, 李继康, 许文贺, 沈沐宇, 戚磊一, 郑可盈, 李伟, 魏青松 |
|
Effects of Overlapping Process on Grain Orientation and Microstructure of Nickel-Based Single-Crystal Superalloy DD491 Fabricated by Selective Laser Melting |
| ZHANG Zhenwu, LI Jikang, XU Wenhe, SHEN Muyu, QI Leiyi, ZHENG Keying, LI Wei, WEI Qingsong |
| 图7 多道搭接熔池示意图和熔池几何特征与工艺参数的关系 |
| Fig.7 Schematic of multi-track overlapping melt pool (a); relationships between process parameters and standard deviation (SD) (b), average melt pool depth ( |
|