铸态及激光粉末床熔融AlCoCrFeNi2.1 共晶高熵合金的微观组织及力学性能 |
| 唐旭, 张昊, 薛鹏, 吴利辉, 刘峰超, 朱正旺, 倪丁瑞, 肖伯律, 马宗义 |
|
Microstructure and Mechanical Properties of As-Cast and Laser Powder Bed Fused AlCoCrFeNi2.1 Eutectic High-Entropy Alloy |
| TANG Xu, ZHANG Hao, XUE Peng, WU Lihui, LIU Fengchao, ZHU Zhengwang, NI Dingrui, XIAO Bolv, MA Zongyi |
| 图10 铸态和LPBF成形AlCoCrFeNi2.1样品在不同温度下拉伸断裂后断口纵截面的SEM像 |
| Fig.10 SEM images of fracture longtudinal sections of as-cast (a, c, e) and LPBF-formed (b, d, f) AlCoCrFeNi2.1 samples after tensile fracture at 20oC (a, b), 500oC (c, d), and 700oC (e, f) |
|