超快激光诱导
Cu
薄膜熔化的神经网络分子动力学研究
高天雨, 曾启昱, 陈博, 康冬冬, 戴佳钰
Neural Network Molecular Dynamics Study of Ultrafast Laser-Induced Melting of Copper Nanofilms
GAO Tianyu, ZENG Qiyu, CHEN Bo, KANG Dongdong, DAI Jiayu
Iter
Lattice structure
Time / ps
Ensemble type
Temperature / K
Pressure / GPa
Sampled configuration
38
Liquid
4
NVT
3000
60
39
Liquid
8
NVT
3000
60
40
fcc
2
NPT
300, 500, 800,
1000, 1200, 1500
0, 1, 5, 10
600
41
fcc
4
NPT
300, 500, 800,
1000, 1200, 1500
0, 1, 5, 10
600
42
fcc
8
NPT
300, 500, 800,
1000, 1200, 1500
0, 1, 5, 10
720
43
Liquid
2
NPT
1500, 2000, 2500, 3000
0, 1, 5, 10
600
44
Liquid
4
NPT
1500, 2000, 2500, 3000
0, 1, 5, 10
600
45
Liquid
8
NPT
1500, 2000, 2500, 3000
0, 1, 5, 10
600