超快激光诱导Cu薄膜熔化的神经网络分子动力学研究 |
| 高天雨, 曾启昱, 陈博, 康冬冬, 戴佳钰 |
|
Neural Network Molecular Dynamics Study of Ultrafast Laser-Induced Melting of Copper Nanofilms |
| GAO Tianyu, ZENG Qiyu, CHEN Bo, KANG Dongdong, DAI Jiayu |
| 图3 不同压强条件下Cu熔点的DP模型结果与实验结果[ |
| Fig.3 DP model results and experimental results of Cu melting point under different pressure conditions (The red dots are the melting points under different pressure conditions calculated using DP, the red curve is the melting curve fitted using Simon-Glatzel equation[ |
|